Rubber & Plastic Products

Most Natural Pigments Survive PLA and PBS Compounding, but Light Stability Limits Use

Mirela ConstantinNovember 2, 20265 min read15 views

At a glance

  • A study finds that most of four natural pigments can be compounded into PLA and PBS on conventional equipment, while thermal sensitivity and UV-driven color change limit broader use.
  • Researchers produced masterbatches from blue spirulina, yellow curcumin, red beetroot and green chlorophyllin in PLA and PBS, and found limited changes in melt flow and mechanical performance at 2–6 wt% masterbatch loadings. However, spirulina lost its blue color during PLA processing, and most formulations showed perceptible color change after 50 hours of xenon exposure.
Four colored biopolymer masterbatch strands—blue, yellow, red and green—coiled beside white PLA and PBS pellets on a laboratory bench, with processing equipment in the background.

Natural colorants are being examined as an alternative to conventional pigments in biodegradable plastics, but they must survive melt processing. A study examined four commercial natural pigments—blue spirulina, yellow curcumin, red beetroot and green chlorophyllin—in polylactic acid (PLA) and polybutylene succinate (PBS). The researchers produced color masterbatches by twin-screw extrusion, diluted them into the corresponding polymer matrices at 2, 4 and 6 wt%, and made test specimens by injection molding. The masterbatch formulation also included titanium dioxide, calcium carbonate and stearic acid to support UV protection, dispersion and processing.

Thermal limits shape compatibility

Heat is a central challenge because the organic pigments can begin to degrade at lower temperatures than the polymers. Thermogravimetric analysis found degradation onset temperatures of about 229°C for spirulina, 244°C for curcumin, 258°C for chlorophyllin and 267°C for beetroot. PLA and PBS showed considerably higher degradation temperatures. The researchers therefore selected extrusion profiles that melted each polymer while limiting the pigments’ thermal exposure. Processing temperatures reached 145°C for PBS and 190°C for PLA, with the twin-screw extruder running at 65 rpm and a feed rate of 2 kg/h.

The window suited most pigment–polymer combinations, but spirulina was a notable exception. During PLA processing it lost its characteristic blue color, preventing production of a blue PLA masterbatch. PBS’s lower processing temperature preserved enough pigment stability for successful compounding. The result indicates that pigment compatibility depends strongly on the thermal requirements of the polymer matrix.

Limited changes to processing and properties

From a processing perspective, the natural pigments caused only limited changes in rheological behavior. Melt flow rate decreased slightly after incorporation, indicating a modest increase in melt viscosity. Neat PLA showed an MFR of about 50 g/10 min, and the corresponding natural-pigment masterbatches stayed close to that value. PBS showed a similar response, with only a minor reduction in melt flow rate.

That matters for compounders because a natural color system has little practical value if it forces major changes to screw design, pressure settings or molding conditions. In the study, conventional twin-screw compounding and injection molding handled most formulations without major processing problems.

The researchers also checked tensile and impact behavior across the 2 to 6 wt% addition range. Neither PLA nor PBS showed significant losses in overall mechanical performance. PLA started with a Young’s modulus of about 1710 MPa and tensile strength of 65.6 MPa; PBS started at about 392 MPa and 34.5 MPa. The colored formulations stayed close to those baselines. Impact strength also remained within a similar range, although individual pigments produced some variation.

Photostability remains the main barrier

Successful extrusion did not ensure long-term color stability. After 50 hours of xenon-lamp exposure, most formulations showed a color difference above Delta E* = 2, indicating a visually perceptible change. The PLA formulation containing 2 wt% green chlorophyllin masterbatch showed the highest photostability and remained the main exception.

The study therefore points to UV stability as the largest barrier to broader use. Packaging, consumer products, agricultural parts and outdoor applications may require additional stabilization, protective coatings or pigment modification before natural colors can compete with conventional systems over long service periods.

The environmental comparison also favored the natural pigments under the study’s assumptions. One kilogram of curcumin pigment generated about 0.04 kg CO2-eq, compared with 18.65 kg CO2-eq for the inorganic green reference pigment. The natural-pigment masterbatches also consumed less electricity during extrusion and pelletizing.

Natural pigment masterbatches still require further development, particularly in lightfastness and thermal stability. Nevertheless, the study demonstrates that several natural colorants can be compounded into PLA and PBS using conventional processing equipment, with only limited changes in melt viscosity and mechanical performance. Future development should focus on improving color stability during processing and subsequent service exposure.

Reported by Mirela Constantin, Industrial Seals and Hoses Analyst.