Renewable Energy

Emulsion buffer limits screen-printing degradation in copper-plated HJT cells, study finds

Dawit BekeleNovember 15, 20265 min read1 views

At a glance

  • A Chinese research team identified worn screen-mesh knuckles as a main cause of damage and found 4.7% emulsion coverage to be the best protection-uniformity trade-off.
  • Researchers in China have identified progressive wear of screen-mesh knuckles as a main cause of efficiency loss when screen-printing photoresist on copper-plated HJT cells. An emulsion buffer layer at 4.7% coverage limited minority-carrier-lifetime degradation to 0.41% after 10,000 printing cycles while maintaining relatively good resist uniformity.
A conceptual close-up shows a screen-printing mesh above a silicon wafer, with a thin emulsion layer keeping the mesh knuckles from direct contact with the cell surface.

Researchers in China have examined how screen printing can degrade copper-plated silicon heterojunction (HJT) solar cells and have proposed a modified screen design to reduce the damage. The study identifies progressive wear of the screen mesh knuckles as a main cause, because worn knuckles increase contact area with the wafer and place greater mechanical stress on sensitive passivation layers.

The work focuses on the photoresist-printing step used in copper plating, not on conventional silver-paste printing. Corresponding author Lang Zhou said the two processes differ in a key way: silver-paste screens have openings covering only 2–5% of the total area, with an emulsion layer covering the rest and preventing direct contact between mesh and wafer. Full-area photoresist coating typically uses a screen without emulsion coverage so the resist can be deposited uniformly across the wafer. As a result, the mesh comes into direct and extensive contact with the wafer during every printing cycle.

Efficiency loss traced to mesh wear

Previous investigations cited by the team found that conversion efficiency declined from 26.2% to 25.7% over 15,000 consecutive printing cycles in commercial solar cell production. Open-circuit voltage and fill factor accounted for most of the loss, while short-circuit current density and electrical resistance remained largely unchanged. Minority-carrier-lifetime degradation rose from 0.61% with a new screen to 11.0% after 15,000 cycles.

Using three-dimensional confocal microscopy, the researchers identified progressive wear of the screen mesh knuckles as the main cause. As the knuckles wore down, their contact area with the wafer grew, increasing mechanical stress on the passivation layers beneath. Scanning electron microscopy showed no visible surface scratches, but photoluminescence measurements indicated higher recombination losses. The team says the result suggests damage at the amorphous-silicon/crystalline-silicon interface.

Emulsion buffer and a coverage trade-off

To prevent direct contact between mesh and wafer, the researchers developed an emulsion buffer layer and evaluated six patterns with emulsion coverage ratios from 2.9% to 16.6%. The results showed a trade-off: greater emulsion coverage provided more mechanical protection but impaired photoresist coating uniformity and ink distribution.

A coverage ratio of 4.7% gave the best balance in the study. At that level, minority-carrier-lifetime degradation was limited to 0.41% after 10,000 printing cycles, while coating uniformity remained relatively good. The improvement was attributed to the emulsion layer keeping the mesh away from the wafer surface and thereby reducing cumulative mechanical damage to the passivation layers.

“The findings demonstrate that a relatively simple modification to screen design can substantially mitigate printing-induced degradation, offering a practical approach to improving the manufacturing reliability of copper-plated HJT solar cells,” Zhou said.

The results were published in Solar Energy in a paper titled “Screen-printing photoresist induced efficiency degradation and mitigation in Cu-plated SHJ solar cells”. The work adds to broader efforts to replace silver contacts in HJT cells with copper metallization, which could lower metallization costs and reduce silver consumption.

Separate recent work illustrates that direction. Researchers at China’s Nankai University reported a silver-free HJT cell with 25.2% efficiency using plasma-induced interface engineering and copper electroplating, addressing adhesion, contact resistance and stability at the ITO interface. At Germany’s Forschungszentrum Jülich, scientists achieved 23.08% efficiency in a fully copper-metallized HJT cell, a relatively small penalty versus a silver-metallized counterpart; cells combining silver-copper paste on the front and silver contacts on the rear reached 23.95%. The findings indicate copper’s potential to cut silver use, although further improvements in processing and electrical performance are still needed.

Reported by Dawit Bekele, Flow, Level and Utility Meter Specialist.